Structure and the metal-support interaction of the Au/Mn oxide catalysts

2010

Gold catalysts with loading 1 and 10 wt % were-prepared by deposition precipitation method with urea over mesoporous manganese oxide, obtained through a surfactant-assisted procedure by using cetyltrimethylammonium bromide (CTAB), followed by treatment with sulphuric acid. For comparison, Au(10 wt %) was also deposited over commercial CeO2 and SiO2 supports. The materials were characterized by XRD and EXAFS at the Mn K and Au L-III edges and XPS. Moreover, the analyses were performed on the samples treated under 1%CO/He, at 250 degrees C for 90 min. The structural and surface results of the as prepared manganese oxide confirmed the formation of gamma-MnO2 along with some amorphous Mn3O4 upo…

Materials scienceGeneral Chemical EngineeringInorganic chemistryTEMPERATURE CO OXIDATIONOxideBixbyiteAEROBIC ALCOHOL OXIDATIONCatalysisMetalENHANCED ACTIVITYchemistry.chemical_compoundX-ray photoelectron spectroscopyBromideMANGANESE OXIDERAY-ABSORPTION SPECTROSCOPYBODY DISTRIBUTION-FUNCTIONSMaterials ChemistryCONDENSED MATTERCERIAGeneral ChemistryTEMPERATURE CO OXIDATION; RAY-ABSORPTION SPECTROSCOPY; BODY DISTRIBUTION-FUNCTIONS; AEROBIC ALCOHOL OXIDATION; GOLD NANOPARTICLES; NANOCRYSTALLINE CEO2; ENHANCED ACTIVITY; CONDENSED MATTER; MANGANESE OXIDE; CERIAchemistryvisual_artGOLD NANOPARTICLESNANOCRYSTALLINE CEO2visual_art.visual_art_mediumMesoporous materialHausmannite
researchProduct